CarSIK-G

CarSIK-G




Bulk density (g/cm3)
3.09
Apparent porosity ( Vol. %)
0
Modulus of rupture / 4-point loading (MPa)
280
Weibull modulus
10
Compressive strengths (MPa)
1,000
Modulus of elasticity (GPa)
360
Vickers hardness (MPa)
SiC 2,5000
Si 9,000
Thermal expansion 20°-1,000°C
Coefficient (1/°C)
4,9 x 10-6
Thermal conductivity (W/mK) 100°C
1,200°C
160
24
Specific heat (J/kgK) RT
1,300°C
600
1,200
Limit of application (°C)
1,380
[1,380]
Chemical composition (wt.%)
SiC
free Si

88
11

The values quoted were determined on test specimens and cannot generally be applied to all shapes.

Picture:
Microstructure CarSIK-G
Dark phase = SiC
Light phase = freies Si